ASME BPVC Section II · SA-1017/SA-1017M Bilingual Technical Reference · 中文 / English
铬 Cr1.90–11.50%按牌号分档
钨 W0.90–2.50%固溶强化
钼 Mo0.05–1.10%高温强化
磷 P / 硫 S≤0.020–0.030%按牌号控制
熔炼分析 / Heat Analysis

四个牌号化学成分限值Chemical Composition Limits, wt%

下表为按公开标准文本整理的熔炼分析(heat analysis)限值;成品分析(product analysis)允许偏差按标准相应条款执行。

表 1 SA-1017/SA-1017M 化学成分(熔炼分析,wt%) / Heat composition limits
元素 ElementGrade 23Grade 911Grade 92Grade 122
碳 C0.04–0.100.09–0.130.07–0.130.07–0.14
锰 Mn0.10–0.600.30–0.600.25–0.66≤0.70
磷 P,max0.0300.0200.0200.020
硫 S,max0.0100.0100.0100.010
硅 Si≤0.500.10–0.50≤0.50≤0.50
铬 Cr1.90–2.608.50–9.508.50–9.5010.00–11.50
钼 Mo0.05–0.300.90–1.100.30–0.600.25–0.60
镍 Ni,max0.400.400.400.50
钨 W1.45–1.750.90–1.101.50–2.001.50–2.50
钒 V0.20–0.300.18–0.250.15–0.250.15–0.30
铌 Nb(Cb)0.02–0.080.06–0.100.04–0.090.04–0.10
氮 N——0.025–0.0750.040–0.100
硼 B0.0009–0.007—0.0009–0.007≤0.005
铝 Al,max0.0400.0400.0400.040
钛 Ti,max0.0100.0100.0100.010
锆 Zr,max0.0100.0100.0100.010

注:“—”表示该牌号在公开整理资料中未单列限值或不做规定;表中数据为工程参考,精确限值、成品分析偏差及残余元素合计要求以现行标准正本 Table 1 与供货质保书为准。

元素作用 / Element Functions

合金元素在耐热钢中的作用Why Each Element Is Added

铬 Cr提高高温抗氧化与耐蚀性,形成表面氧化膜;含量决定牌号档位。
钼 Mo固溶强化基体,提高高温蠕变强度与抗氢腐蚀能力。
钨 W以固溶方式强化并改善持久性能,是本标准区别于普通 Cr-Mo 钢的特征元素。
钒 V / 铌 Nb形成稳定碳氮化物,细化晶粒并抑制高温长期服役中的组织粗化。
氮 N在 92、122 牌号中配合钒铌析出强化,稳定马氏体/铁素体基体组织。
碳 C保证强度与淬硬倾向的平衡;含量上限直接影响焊接性与韧性。
磷 P / 硫 S杂质元素,上限受控以降低脆性与热裂倾向。
硼 B微量偏聚于晶界改善淬透性与高温性能,含量控制在很小范围内。
核对要点 / Checks

成分核对时容易忽略的条款Items Easy to Miss

熔炼与成品分析Heat vs Product Analysis

标准同时规定熔炼分析与成品分析限值;订货验收应以质保书载明的分析类别和取样位置为准。

残余元素控制Residual Elements

镍、铜、铝、钛、锆等元素有上限或合计控制要求;废料来源不明的材料应增加光谱复验。

微合金元素Microalloys

氮、硼含量区间窄,对热处理与韧性敏感;重要部件应核对熔炼报告中的实测值而非仅看牌号。

合规提示:本站成分表用于选材沟通与资料整理,不构成材料验收结论;正式设计、订货与复验须以标准正本、技术协议和第三方检验结果为准。

关键词 / Keywords

电话咨询 Call 邮件询价 Inquiry