化学成分 Chemical Composition
质量分数(%);下表为熔炼分析(heat analysis)限值,成品分析(product analysis)允许规范规定的偏差。
| 元素 Element | Gr.2 | Gr.12 | Gr.11 | Gr.22 | Gr.21 | Gr.5 | Gr.9 | Gr.91 |
|---|---|---|---|---|---|---|---|---|
| 碳 C | 0.05–0.21 | 0.05–0.17 | 0.05–0.17 | 0.05–0.15 | 0.05–0.15 | ≤0.15 | ≤0.15 | 0.08–0.12 |
| 锰 Mn | 0.55–0.80 | 0.40–0.65 | 0.40–0.65 | 0.30–0.60 | 0.30–0.60 | 0.30–0.60 | 0.30–0.60 | 0.30–0.60 |
| 硅 Si | 0.15–0.40 | 0.15–0.40 | 0.50–0.80 | ≤0.50 | ≤0.50 | ≤0.50 | ≤1.00 | 0.20–0.50 |
| 磷 P,≤ | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.020 |
| 硫 S,≤ | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.010 |
| 铬 Cr | 0.50–0.80 | 0.80–1.15 | 1.00–1.50 | 2.00–2.50 | 2.75–3.25 | 4.00–6.00 | 8.00–10.00 | 8.00–9.50 |
| 钼 Mo | 0.45–0.60 | 0.45–0.60 | 0.45–0.65 | 0.90–1.10 | 0.90–1.10 | 0.45–0.65 | 0.90–1.10 | 0.85–1.05 |
注 1:厚度大于 125 mm(5 in.)的 Gr.22、Gr.21 钢板,成品分析碳含量上限为 0.17%。注 2:Grade 91 Type 2 的 Mn 上限为 0.50%、Si 为 0.20–0.40%、S 上限为 0.005%,Mo 成品分析为 0.80–1.05%;以标准正本为准。
Grade 91 微合金元素(参考 Table 1)Micro-alloying Elements
| 钒 V | 铌 Nb | 氮 N | 镍 Ni,≤ | 铝 Al,≤ | 钛 Ti,≤ |
|---|---|---|---|---|---|
| 0.18–0.25 | 0.06–0.10 | 0.030–0.070 | 0.40 | 0.02 | 0.01 |
铬 Cr
提高高温抗氧化、抗腐蚀与抗氢侵蚀能力;含量随牌号由 0.5% 级提高至 9% 级。
钼 Mo
固溶强化并改善高温蠕变(creep)性能,是铬钼耐热钢的核心强化元素之一。
钒 V / 铌 Nb / 氮 N
Grade 91 借助 V、Nb、N 形成细小碳氮化物析出强化,改善长期高温强度。
磷 P / 硫 S
有害杂质元素,按规范限量控制;临氢与厚壁容器通常进一步降低 P、S 及 Sn、Sb、As 等残留元素。